    • PUBLICATION

    PAPER

    Influence of Aqueous Carboxymethyl Cellulose Binder Viscosity on the Anode Performance in Lithium Ion Batteries
    관리자
    2024-03-13      조회 944   댓글 0  
    Author Hyunchul Kang, Eunsun Shin, Keebum Hwang, Jaekwang Kim, Songhun Yoon
    Journal 폴리머
    Year of Pub. 2022


    Influence of Aqueous Carboxymethyl Cellulose Binder Viscosity on the Anode Performance in Lithium Ion Batteries

    Viscosity effect of carboxymethyl cellulose (CMC), an aqueous binder for lithium secondary batteries, on the electrochemical performance of graphite anode materials is investigated by changing the adhesion to graphite, binder, and current collector. Using three CMC binders with different molecular weight, viscosity of pure aqueous solutions and anode slurry solutions with graphite materials are compared using rheometer. The rheological trend is dependent on the interaction between CMC binder and graphite material. After fabrication of the anodes in lithium ion batteries , the binder with highest viscosity showed the best cycle and rate performances; 88.0% @ 140 cycles and 220.6 mA h g−1 @ 2C rate, which is attributed to high adhesion strength with current collector. Furthermore, formation of different microstructures results in advanced cycle performance and low rate capability (86.3% after 140 cycles) from the enhanced viscosity slurry solution in spite of weak adhesion property with current collector. Hence, the rheology of the slurry solution can critically influence on the electrochemical performance of the graphite anode in LIBs.
    첨부파일 97.PNG (210.21KB) [0] 2024-03-13 17:12:50
    이전글 Ni-rich cathode material with isolated porous layer hindering crack propagation under 4.5 V high cut-off voltage cycling
    다음글 State of health monitoring by gas generation patterns in commercial 18,650 lithium-ion batteries